发明名称 Non-heat treated steel for soft-nitriding
摘要 Non-heat treated steel for soft-nitriding to form parts having high fatigue strength and excellent bend leveling property even in a case of applying soft-nitriding without thermal refining, comprising, by mass %, C: 0.30 to 0.45%, Si: 0.1 to 0.5%, Mn: 0.6 to 1.0%, Ti: 0.005-0.1% and N: 0.015 to 0.030%, and the balance Fe and impurities, having a mixed microstructure of bainite and ferrite whose bainite fraction is 5 to 90% or having a mixed microstructure of bainite, ferrite and pearlite whose bainite fraction is 5 to 90%, the steel could contain one or more of elements of Nb: 0.003 to 0.1% Mo: 0.01 to 1.0%, Cu: 0.01-1.0%, Ni: 0.01 to 1.0%, B: 0.001 to 0.005%, S: 0.01 to 0.1%, and Ca: 0.0001 to 0.005.
申请公布号 US7416616(B2) 申请公布日期 2008.08.26
申请号 US20050312498 申请日期 2005.12.21
申请人 SUMITOMO METAL INDUSTRIES, LTD. 发明人 SANO NAOYUKI;NAKATANI TAKAYUKI;KAMADA YOSHIHIKO
分类号 C22C38/22;C22C38/00;C22C38/04;C22C38/14;C22C38/60 主分类号 C22C38/22