发明名称 METHODS FOR FORMING AMORPHOUS ULTRA-HIGH MOLECULAR WEIGHT POLYALPHAOLEFIN DRAG REDUCING AGENTS
摘要 A composition including polyalphaolefins that function as drag reducing agen ts and a process for the preparation of polyalphaolefins that function as drag reducing agents are disclosed. The process includes contacting alpha olefin monomers with a catalyst system, which includes a catalyst and an activator (co-catalyst) in a reactant mixture. The catalyst is a transition metal catalyst, preferably titanium trichloride, and the co-catalyst may include a n alkylaluminoxane, alone or in combination, with a dialkylaluminum halide or a halohydrocarbon. The polymerization of the alpha olefin monomers produces a non-crystalline, ultra-high molecular weight polyalphaolefin having an inherent viscosity of at least 10 dL/g. The addition of the alkylaluminoxane during the polymerization process provides for a non-crystalline, ultra-high molecular weight polyalphaolefin and a more uniform molecular weight distribution of the resulting polyalphaolefin, thereby creating a drag reducing agent superior to known drag reducing agents. A process for forming a drag reducing agent comprising a non-crystalline, ultra-high molecular weigh t polyalphaolefin having an inherent viscosity of about at least 10 dL/g and a process for reducing drag in a conduit are also disclosed.
申请公布号 CA2332716(C) 申请公布日期 2008.08.05
申请号 CA19992332716 申请日期 1999.05.14
申请人 ENERGY & ENVIRONMENTAL INTERNATIONAL, L.C. 发明人 EATON, GERALD B.;MONAHAN, MICHAEL J.;TIPTON, ROBERT J.
分类号 C08F210/14;C08F2/00;C08F2/08;C08F2/42;C08F2/44;C08F4/44;C08F4/642;C08F4/649;C08F10/00;C08F110/00;C08F210/00;C08F210/16;C08J5/16;C08L23/00;C09K3/00;C10L1/16;C10M107/10;C10M143/08;F17D1/16 主分类号 C08F210/14
代理机构 代理人
主权项
地址