摘要 |
A polyester for a toner having a softening point of from 70° to 110° C. and a glass transition temperature of from 38° to 60° C., obtained by polycondensing an alcohol component containing a propylene oxide adduct of bisphenol A and an ethylene oxide adduct of bisphenol A in a total amount of 80% by mole or more, with a carboxylic acid component, wherein the propylene oxide adduct has an average number of moles of from 2.0 to 2.4, and the ethylene oxide adduct has an average number of moles of from 2.5 to 4.2. The polyester for a toner of the present invention is suitably used as a resin binder of a toner, or the like, used for, for example, developing a latent image formed in electrophotography, electrostatic recording method, electrostatic printing method, or the like.
|