摘要 |
Thermoplastic polyurethanes are obtainable by reacting (a) isocyanates with (b1) polyesterdiols having a melting point greater than 150-C, (b2) polyetherdiols and/or polyesterdiols, each having a melting point of less than 150-C and a molecular weight of from 501 to 8 000 g/mol, and, if required, (c) diols having a molecular weight of from 62 to 500 g/mol.
|