摘要 |
PROBLEM TO BE SOLVED: To provide a woven fabric developing no wrinkles under flat-iron or in a press step, having high stretchability and improved in touch feeling as well. SOLUTION: The fabric has at least one of warps and wefts in which polytrimethylene terephthalate fiber-containing yarns and polyethylene terephthalate false-twist textured yarns are arranged, and a difference in crimp elongation rate (CRZ) between the polytrimethylene terephthalate fiber-containing yarn and the polyethylene terephthalate false-twist textured yarn meets the relationship: 30≥CRZ(%)≥5. COPYRIGHT: (C)2008,JPO&INPIT
|