发明名称 Compositions comprising acrylonitrile polymers and copolymers and shaped articles produced therefrom
摘要 Compositions suitable for making yarns, films and shaped articles comprise a solution of polyacrylonitrile or of a copolymer in which at least 85 per cent by weight is acrylonitrile, in a solvent comprising a compound from a specified class of cyclic organic sulphoxy compounds containing a 4-7 membered ring structure. The compositions are clear mobile solutions at elevated temperatures, e.g. 100 DEG C., and may gel at room temperature. The preferred compounds are methoxytetramethylene sulphone and tetramethylene sulphoxide, but others specified are substituted with oxygen, sulphur, nitrogen, halogen, hydroxy, thiol, methyl and methoxy groups, e.g. 1.4-thioxane-4-oxide, pentamethylene sulphone, b -aminotetramethylene sulphone, b -mercapto-tetramethylene sulphone, tetrahydro-1.4-thiopyrone-1.1-dioxide, divinylene disulphide-1.1-dioxide, 1.4-thiazane-4-oxide and b -bromotetramethylene sulphone. Specified compounds with which the acrylonitrile may be copolymerized are vinyl and acrylic compounds, isobutylene and butadiene (see Group V). Optionally, the compositions may contain other plasticisers (non-solvents for the polymer), e.g. glycerol, solvents for the polymer of lower b.p., and dyes, linear polyamides, cellulose ethers and esters, polyvinyl chloride and acetate and polyacrylic acid. The solutions may be shaped to form filaments, yarns, films, tubes and other articles, e.g. by moulding, casting or extrusion into an evaporative atmosphere or a bath of coagulant miscible with the solvent but an inert non-solvent for the polymer, e.g. water, glycerol, alcohol, ether and aqueous solutions of salts, alkalies and acids. The properties of the products can be improved by subjecting them to a stretching operation. The solutions are also suited for use as lacquers and coating compositions e.g. as coatings for wires. The dry and wet spinning of yarn and the casting of films from the compositions is described. The yarn is drawn by the method of Specification 585,368. Specifications 404,504, 579,887 and 594,999, and U.S.A. Specifications 2,117,210, 2,140,921 and 2,167,537 also are referred to.ALSO:Compositions suitable for making yarns, films and shaped articles comprise a solution of polyacrylonitrile or of a copolymer in which at least 85 per cent. by weight is acrylonitrile, in a solvent comprising a compound from a specified class of cyclic organic sulphoxy compounds containing a 4-7 membered ring structure [see Group IV]. The compositions are clear mobile solutions at elevated temperatures, e.g., 100 DEG C, and may gel at room temperature. The preferred compounds are p methoxy-tetramethylene sulphone and tetramethylene sulphoxide, but others specified are substituted with oxygen, sulphur, nitrogen, halogen, hydroxy, thiol, methyl and methoxy groups, e.g., 1.4-thioxane-4-oxide, pentamethylene sulphone, b -amino-tetramethylene sulphone, b -mercapto-tetramethylene sulphone, tetrahydro-1.4-thiopyrone-1.1-dioxide, divinylene disulphide-1.1-dioxide, 1.4-thiazane-4-oxide and b -bromotetramethylene sulphone. The acrylonitrile may be copolymerised with diolefines, e.g., butadiene. Optionally, the compositions may contain other plasticizers (non-solvents for the polymer), e.g., glycerol, solvents for the polymer of lower b.p., and dyes, linear polyamides, cellulose ethers and esters, polyvinyl chloride and acetate and polyacrylic acid. The solutions may be shaped to form filaments, yarns, films, tubes and other articles, e.g., by moulding, casting or extrusion into an evaporative atmosphere or a bath of coagulant miscible with the solvent but an inert non-solvent for the polymer, e.g., water, glycerol, alcohol, ether and aqueous solutions of salts, alkalies and acids. The properties of the products can be improved by subjecting them to a stretching operation. The solutions are also suited for use as lacquers and coating compositions, e.g., as coatings for wires. The dry and wet spinning of yarn and the casting of films from the compositions is described. The yarn is drawn by the method claimed in Specification 585,368, [Group IV]. Specifications 404,504, 579,887 and 594,999, [all in Group IV], and U.S.A. Specifications 2,117,210, 2,140,921 and 2,167,537 also are referred to.
申请公布号 GB595050(A) 申请公布日期 1947.11.25
申请号 GB19450029120 申请日期 1945.11.02
申请人 E. I. DU PONT DE NEMOURS AND COMPANY 发明人
分类号 C08J3/09;C08K5/45;D01D5/12;D01F6/18 主分类号 C08J3/09
代理机构 代理人
主权项
地址