in a process for preparing polyethylene waxes at from 200 to 350.degree.C and pressures in the range from 500 to 4 000 bar using molar mass regulators, a peroxide mixture comprising from 5 to 95% by weight of at least one cyclic peroxide of the formula 1, <IMG> where the radicals R are identical or different and are selected from among alkyl groups and aryl groups, is used as free radical initiator and a molar H2/ethylene ratio of from 1:2 000 to 1:40 000 is employed.
申请公布号
CA2341008(C)
申请公布日期
2008.05.06
申请号
CA20012341008
申请日期
2001.03.15
申请人
WITTKOWSKI, LARS;MAHLING, FRANK-OLAF;WEBER, WILHELM;DECKERS, ANDREAS
发明人
WITTKOWSKI, LARS;MAHLING, FRANK-OLAF;WEBER, WILHELM;DECKERS, ANDREAS