摘要 |
A functional particle is manufactured by a method including an aggregating step, a depressurizing step, and a cooling step. In the aggregating step, the functional particle is obtained by flowing a mixed slurry containing a core particle and a shell particle through a coiled pipeline while heating the mixed slurry to a glass transition temperature or higher of the core particle, to deposit the shell particles on the surface of the core particle. In the depressurizing step, the grain size of the functional particle is controlled and the coarse particle is pulverized to make the grain size of the functional particles uniform. In the cooling step, re-aggregation of the functional particles with unified grain size is prevented.
|