摘要 |
<p>A process is disclosed for obtaining colloid-forming metal particles from an aqueous mine waste solution containing that metal in ionic form. In accordance with this process, an aqueous mine waste solution containing that metal in ionic form is provided having a pH value of about 4.0 to about 6.5. The solution is electrified with direct current at about 1.2 to about 2.0 volts to reduce the desired metal ions to colloidal metal particles. A slurry of cellulose particles is agitatingly added to the colloid composition followed by a flocculant to form a solid phase cellulosic floc containing the colloid. The solid and liquid phases are separated, and the solid phase is dried, fluxed and heated to a temperature sufficient to melt the flux and colloid and form larger metal particles that can then be recovered. The colloid-forming metal is preferably gold.</p> |