摘要 |
A method of making a solution of a polyimide from a diamine monomer and a dianhydride monomer is disclosed. A solution or slurry of one of the monomers in a solvent that boils at a temperature between about 80° C. and about 160° C. is prepared. The solution or slurry is heated to a temperature between about 80° C. and about 160° C. and the other monomer is slowly added to the solution or slurry. Polyamic acid that is formed quickly imidizes to form the polyimide. |