发明名称 GLASFASERGRANULAT MIT HOHER DICHTE
摘要 <p>The preparation of glass fibre granules is carried out by mixing cut glass fibres, sized using a size comprising an organosilane, in the presence of 10 to 25 % water for a sufficient time such that the density increases by at least 67 % using a single mixing device which mixes the fibres or granules constantly at the same frequency. The preparation of glass fibre granules is carried out by mixing cut glass fibres, sized using a size comprising an organosilane, in the presence of 10 to 25 % water for a sufficient time such that the density increases by at least 67 % using a single mixing device which mixes the fibres or granules constantly at the same frequency. After drying, the final granules formed contain at least 95 wt.- % glass. A tackifying agent is in contact with the glass fibres at the latest during the mixing. Independent claims are also included for: (a) Glass fibre granules, with a diameter of between 1 and 10 mm and comprising 50,000 to 500,000 glass filaments, obtained by this method; (b) utilization of these granules for reinforcing a thermoplastic.</p>
申请公布号 DE60314249(T2) 申请公布日期 2008.01.31
申请号 DE2003614249T 申请日期 2003.05.21
申请人 SAINT-GOBAIN VETROTEX FRANCE S.A. 发明人 BLANCHARD, JEAN-FRANCOIS;VIANA, JEAN-LOUIS;BASTARD, MICHEL;FONT, DOMINIQUE
分类号 C03B37/14;C08J5/08;C03B37/16;C03C1/02;C03C25/26;C08K7/14 主分类号 C03B37/14
代理机构 代理人
主权项
地址
您可能感兴趣的专利