发明名称 СПОСОБ ПОЛУЧЕНИЯ ЛИТЕЙНЫХ АЛЮМИНИЕВО-КРЕМНИЕВЫХ СПЛАВОВ
摘要 FIELD: non-ferrous metallurgy; production of aluminum-silicon alloys, silumines, for example. ^ SUBSTANCE: used as burden is primary silumine, returns of sand-clay casting and returns of permanent-mold casting process at mass ratio of (1-1.6): (2.3-3.6) : (2-2.6). Part of burden containing primary silumine and returns of sand-clay casting process is molten and melt is overheated to temperature of 1000-1050°C, after which it is cooled down to temperature of 825-875°C due to introduction of first portion of returns of permanent-mold casting process in the amount of 60-70% of their mass; then remaining returns of permanent-mold casting process are charged for obtaining crystallization centers sufficient for grinding the structure. ^ EFFECT: enhanced mechanical properties of alloy; facilitated procedure due to production of alloy in one unit; avoidance of expensive modifiers. ^ 1 tbl, 1 ex
申请公布号 RU2006123589(A) 申请公布日期 2008.01.20
申请号 RU20060123589 申请日期 2006.07.03
申请人 Государственное образовательное учреждение высшего профессионального образовани  СИБИРСКИЙ ГОСУДАРСТВЕННЫЙ ИНДУСТРИАЛЬНЫЙ УНИВЕРСИТЕТ (RU) 发明人 Дегт рь Валерий Аронович (RU);Деев Владислав Борисович (RU);Сел нин Иван Филиппович (RU);Войтков Алексей Петрович (RU)
分类号 C22C1/02;C22C21/04 主分类号 C22C1/02
代理机构 代理人
主权项
地址