摘要 |
PROBLEM TO BE SOLVED: To provide an aromatic polycarbonate resin composition which gives moldings having a low dimensional change due to thermal expansion even for large-sized ones as well as high rigidity and impact resistance and a good surface appearance and its molding. SOLUTION: The aromatic polycarbonate resin composition contains 50-100 wt.% of (component A) an aromatic polycarbonate resin, 0-50 wt.% of (component B) a thermoplastic resin comprising at least one kind of resin selected from among the group consisting of (component B-1) thermoplastic polyester resins and (component B-2) resins containing a styrene unit component with a rubber component content of less than 40 wt.% and (component C) wollastonite particles having a number-average fiber length of≤10μm, a number-average fiber diameter of≤1.5μm and an aspect ratio as calculated from the number-average fiber length and diameter of≥4.5 in an amount of 1-100 pts.wt. to 100 pts.wt. of the resin components. The molding is obtained from the composition. COPYRIGHT: (C)2008,JPO&INPIT
|