发明名称 ДОБАВКА К ЦЕМЕНТУ
摘要 There are provided a cement admixture which enhances water reducing property and flowability of a cement composition, and is excellent in slump retaining performance to retain the flowability with time, a polycarboxylic acid-based polymer for a cement admixture suitable therefor, a producing method thereof, and a cement composition. One cement admixture of the present invention contains copolymers (A) and (B) as an essential component, weight average molecular weights (AMw and BMw) of copolymers (A) and (B) are AMw > BMw, or peaktop molecular weights (AMp and BMp) of copolymers (A) and (B) are AMp > BMp. Another cement admixture of the present invention contains a polycarboxylic acid-based polymer having a lower molecular weight side area ratio P of 50 to 87%.
申请公布号 RU2006122535(A) 申请公布日期 2008.01.10
申请号 RU20060122535 申请日期 2004.12.28
申请人 НИППОН СОКУБАИ КО., ЛТД. (JP) 发明人 ХВЯСИЯ Тосио (JP);УЕТА Томи су (JP);ЮАСА Цутому (JP);ХИРАТА Цуеси (JP);ЯМАЗАКИ Хироси (JP)
分类号 C04B24/26;C04B28/02;C04B40/00;C04B103/30;C08F220/06;C08F290/06;C08K3/00;C08L55/00 主分类号 C04B24/26
代理机构 代理人
主权项
地址