<p><P>PROBLEM TO BE SOLVED: To provide a regenerated polyolefin-based resin composition that controls stagnation of a low molecular weight resin as a material causing die drool at pointed end of a die of an extruder exit, and gives a good surface condition when molded in a desired shape, and to provide a method for producing the same. <P>SOLUTION: The regenerated polyolefin-based resin composition comprises a polyolefin-based resin, a derivative of a hydroxy-fatty acid amide, and silicon dioxide, and is produced by adding a derivative of the hydroxy-fatty acid amide and silicon dioxide to a polyolefin-based resin having a crosslinking structure, and by melt kneading the mixture loading shearing force while heating above the melting point of the polyolefine-based resin. <P>COPYRIGHT: (C)2008,JPO&INPIT</p> |