发明名称 Cellulose acylate film and method for producing same, and retardation film, polarizing plate and liquid crystal display device comprising the film
摘要 A Cellulose acylate film, in which X-ray diffraction intensity satisfies following formulae and a half-value width of the peak at 2theta<SUB>2 </SUB>is greater than 3° and not greater than 7°: <?in-line-formulae description="In-line Formulae" end="lead"?>0.40<=Ic<SUB>2</SUB>/(Iam<SUB>2</SUB>+Ic<SUB>2</SUB>) <=0.75;<?in-line-formulae description="In-line Formulae" end="tail"?> <?in-line-formulae description="In-line Formulae" end="lead"?>Iam<SUB>2</SUB>I<SUB>1</SUB>+{(I<SUB>3</SUB>-I<SUB>1</SUB>)/(2theta<SUB>3</SUB>-2theta<SUB>1</SUB>)x(2theta<SUB>2</SUB>-2theta<SUB>1</SUB>)}; and<?in-line-formulae description="In-line Formulae" end="tail"?> <?in-line-formulae description="In-line Formulae" end="lead"?>Ic<SUB>2</SUB>=<SUB>2</SUB>-Iam<SUB>2</SUB>,<?in-line-formulae description="In-line Formulae" end="tail"?> wherein when it is assumed that thetais the Bragg angle, 2theta<SUB>1 </SUB>and 2theta<SUB>3 </SUB>indicate 2theta at which the intensity becomes the minimum in the 2theta range of 4° to 5° and 14° to 16°, respectively, 2theta<SUB>2 </SUB>indicates 2theta at which the intensity becomes the maximum in the 2theta range of 5° to 10°, and I<SUB>1</SUB>, I<SUB>2 </SUB>and I<SUB>3 </SUB>indicate a diffractive intensity at 2theta<SUB>1</SUB>, 2theta<SUB>2 </SUB>and 2theta<SUB>3</SUB>, respectively.
申请公布号 US2007269617(A1) 申请公布日期 2007.11.22
申请号 US20070798848 申请日期 2007.05.17
申请人 FUJIFILM CORPORATION 发明人 SASADA YASUYUKI
分类号 C09K19/00 主分类号 C09K19/00
代理机构 代理人
主权项
地址
您可能感兴趣的专利