Alloy powder for forming hard phase and ferriferous mixed powder using the same, and manufacturing method for wear resistant sintered alloy and wear resistant sintered alloy |
摘要 |
Alloy powder for forming a hard phase for a valve seat material having excellent high temperature wear resistance. The overall composition is consisted of Mo: 48 to 60 mass %, Cr: 3 to 12 mass % and Si: 1 to 5 mass %, and the balance of Co and inevitable impurities.
|