摘要 PROBLEM TO BE SOLVED: To provide a construction method strengthening sure adhesive strength between an aggregate and a road surface after a road is opened initially. SOLUTION: The construction method is composed of a process manufacturing primary improved asphalt obtained by adding a resin additive to straight asphalt, a process manufacturing secondary improved asphalt by adding an oil additive to primary improved asphalt and a process 1 adding water to secondary improved asphalt heated to a fixed temperature, agitating and mixing secondary improved asphalt and laying secondary improved asphalt 9 in a foamed state on the road surface. The construction method is further composed of a process 3 scattering the aggregate 17 from the upper section of secondary improved asphalt 9 in the foamed state and a process 5 flatly rolling secondary improved asphalt 9 by a rolling machine 19 after the aggregate is scattered. COPYRIGHT: (C)2008,JPO&INPIT
申请公布号 JP2007277994(A) 申请公布日期 2007.10.25
申请号 JP20060107917 申请日期 2006.04.10
申请人 NIPPON ROAD CO LTD:THE 发明人 TAKEDA TAKESHI;OKABAYASHI MASATOSHI
分类号 E01C7/32;E01C7/22;E01C23/00 主分类号 E01C7/32
代理机构 代理人
主权项
地址