摘要 |
<p>A self-leveling mortar composition is provided to have short setting time, excellent constructability, good flowability, and superior adhesion strength and bending strength. A self-leveling mortar composition is obtained by mixing 30-60wt% of cement, 30-60wt% of sand, 0.1-30wt% of a finely powdered admixture, 0.1-10wt% of a natural inorganic pigment, 0.0001-3.0wt% of fiber, 0.1-5.0wt% of a shrinkage-reducing agent, and 0.05-10wt% of other additive. The other additive is at least one selected from 0.01-2.5wt% of a superplasticizer, 0.01-2.5wt% of a thickener, 0.01-2.5wt% of a retarding agent, and 0.01-2.5wt% of an accelerator.</p> |