<p>Disclosed is a diphenylmethane isocyanate composition comprising a composition which is obtained by adding an alkylchlorosilane having 4-24 carbon atoms in total in the molecular structure to a diphenylmethane isocyanate having an acid degree of less than 0.1% by mass. This diphenylmethane isocyanate composition has a high acid degree of not less than 0.1% by mass. The alkylchlorosilane is preferably 1,3-dichlorotetraisopropyldisiloxane or triethylchlorosilane. The diphenylmethane isocyanate composition takes a longer time before starting to increase in viscosity (namely, has a higher storage stability) than the conventional ones.</p>
申请公布号
WO2007116761(A1)
申请公布日期
2007.10.18
申请号
WO2007JP56466
申请日期
2007.03.27
申请人
NIPPON POLYURETHANE INDUSTRY CO., LTD.;TAKEDA, TAKEO;YAMAGUCHI, TATSUYA;YOSHIHARA, TOMOMITSU;YAMADA, SUSUMU;KANBARA, YOSHIYUKI