摘要 |
PROBLEM TO BE SOLVED: To sufficiently show original lubrication characteristics of solid lubricant and eliminate risk of peeling off of solid lubricant from a base material at an early stage without resin in a sliding member provided with the coating layer comprising solid lubricant. SOLUTION: Supposing the sliding member 4 of a structure adhering the coating layer 8 including a sliding surface on the base material 6, an intermediate layer 7 is provided between the base material 6 and the coating layer 8, and the coating layer 8 has a laminated structure of solid lubricant plate shape crystal particle 3. The lubricant plate shape crystal particle 3 has crystal structure having (001) surface (provided that 1 is an integer of 1 or greater) laminated in parallel and orientation index of the (001) surface is 90% or higher at least on the sliding surface. COPYRIGHT: (C)2008,JPO&INPIT
|