发明名称 REFRACTORY MATERIAL FOR DESILICONIZATION CONTAINER
摘要 <P>PROBLEM TO BE SOLVED: To provide a refractory material for a desiliconization container, having good corrosion resistance and spalling resistance and having a long durability. <P>SOLUTION: A freeboard A and a slag line B in a hot metal ladle for desiliconization are made from a refractory material 15 having a composition of 92 to 30 mass% alumina, 5 to 50 mass% chromia, not more than 10 mass% zirconia, provided that the total amount of alumina, chromia, and zirconia is not less than 90 mass%. <P>COPYRIGHT: (C)2008,JPO&INPIT
申请公布号 JP2007269596(A) 申请公布日期 2007.10.18
申请号 JP20060099753 申请日期 2006.03.31
申请人 TOKYO YOGYO CO LTD 发明人 YOSHIDA TAKESHI;KOIDE KUNIHIRO
分类号 C04B35/66;C21C1/04;C21C1/06;F27D1/00 主分类号 C04B35/66