Known protective layers with a high Cr content and additionally a silicon form brittle phases, which become even more brittle under the influence of carbon during use. The protective layer according to the invention has the composition 27% to 31% nickel, 23% to 29% chromium, 7% to 11% aluminium, 0.5% to 0.7% yttrium and/or at least one equivalent metal from the group comprising scandium and rare earth elements, optionally 0.6% to 0.8% silicon, optionally 0.5% to 0.7% zirconium and the remainder cobalt.
|