摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a polyvinyl glove causing extremely slight elution of a plasticizer even when treating oily food and having a thickness of <0.5 mm and to provide a new polyvinyl-based paste resin composition enabling production of the polyvinyl glove. <P>SOLUTION: The polyvinyl glove having a thickness of 0.25 mm is produced by using the resin composition where 70-120 pts.wt. of a polyester-based plasticizer having an average molecular weight of 3,400, and 60-100 pts.wt. of 2,2,4-trimethyl-1,3-pentadiol diisobutylate (TXIB) are added to 100 pts.wt. of polyvinyl-based paste resin. <P>COPYRIGHT: (C)2008,JPO&INPIT</p> |