Method of forming an outwardly grown aluminide diffusion coating on a superalloy substrate disposed in a coating retort including the steps of heating the substrate to a temperature of 900 to 1200 degrees C., flowing a coating gas comprising aluminum trichloride and a carrier gas through the coating retort at a flow rate of the coating gas of about 100 to about 450 standard cubic feet per hour, providing a concentration of aluminum trichloride in the retort of less than 1.4% by volume of the coating gas, and providing a total pressure of the coating gas in the coating retort of about 100 to about 450 Torr.
|
申请公布号 |
US7273635(B2) |
申请公布日期 |
2007.09.25 |
申请号 |
US20030674059 |
申请日期 |
2003.09.29 |
申请人 |
HOWMET CORPORATION |
发明人 |
PURVIS ANDREW L.;WARNES BRUCE M.;MCFARREN IRVING R.;COCKERILL JOEL L. |
分类号 |
C23C10/28;C23C16/12;C23C8/02;C23C8/06;C23C16/00;C23C16/34;C23C16/40;C23C16/455;C23C28/00 |
主分类号 |
C23C10/28 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|