发明名称 |
ALUMINA CEMENT, ALUMINA CEMENT COMPOSITION AND MONOLITHIC REFRACTORY |
摘要 |
<P>PROBLEM TO BE SOLVED: To provide alumina cement capable of keeping the fluidity for a long time at a low temperature and having high strength and an alumina cement composition and monolithic refractory using the same. <P>SOLUTION: The alumina cement containing CA and C<SB>2</SB>AS as a mineral composition contains 25-40 mass% CaO and 0.01-0.15 mass% potassium expressed in terms of K<SB>2</SB>O. The alumina cement composition contains the alumina cement and aggregate. The monolithic refractory contains the alumina cement and refractory aggregate. <P>COPYRIGHT: (C)2007,JPO&INPIT |
申请公布号 |
JP2007210805(A) |
申请公布日期 |
2007.08.23 |
申请号 |
JP20060029316 |
申请日期 |
2006.02.07 |
申请人 |
DENKI KAGAKU KOGYO KK |
发明人 |
YOSHIOKA MITSUHIRO;UMIGA MASAAKI;KUSHIHASHI KAZUTO |
分类号 |
C04B7/32;C04B14/30;C04B14/32;C04B14/36;C04B28/06;C04B35/66;F27D1/00 |
主分类号 |
C04B7/32 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|