发明名称 METHOD FOR LINEARLY HEATING STEEL SHEET
摘要 PROBLEM TO BE SOLVED: To provide a method for linearly heating a steel sheet, which method can stably achieve a large deformation angle. SOLUTION: The method for linearly heating the steel sheet is used for heating the steel sheet so as to simultaneously satisfy both of the following conditions: 700≤Ts≤1,000; and 27×(IYS/1,000)<SP>0.7</SP>×t<SP>-0.32</SP>-30≤Tr≤27×(IYS/1,000)<SP>0.7</SP>×t<SP>-0.32</SP>+30, where Ts(°C) shows a maximum arrival temperature on the right side surface of the steel sheet in the linear heating; Tr(°C) shows a maximum arrival temperature on the back surface of the steel sheet in the linear heating; IYS(K N/mm<SP>2</SP>) shows an integrated value of the yield strength of the steel sheet with respect to temperature from an ordinary temperature to 600°C; and t(mm) shows the thickness of the steel sheet. COPYRIGHT: (C)2007,JPO&INPIT
申请公布号 JP2007181849(A) 申请公布日期 2007.07.19
申请号 JP20060000782 申请日期 2006.01.05
申请人 NIPPON STEEL CORP 发明人 SHIRAHATA HIROYUKI;KASUYA TADASHI;SHISHIBORI AKIRA
分类号 B21D11/20;C21D8/00;C22C38/00;C22C38/58 主分类号 B21D11/20
代理机构 代理人
主权项
地址