<p>The invention relates to thermoplastic moulding compounds containing A) 35-95 wt. % of at least one graft copolymer A) which can be obtained by reacting A1) 5 -95 wt. % of a polymer A1) which is obtained from at least one dicarboxylic acid anhydride a11) and at least one vinyl aromatic comonomer a)12), and A2) 5 - 95 wt.- % of a polyamide A2), B) 5 - 40 wt % of at least one non-grafted or grafted, particulate rubber without a core-shell structure B),comprising functional groups which can react with terminal groups of component A), C) 0 - 50 wt. % of at least one particulate or fibrous filling or reinforcing material C), D) 0 - 60 wt. % of at least one copolymer D) made of vinylaromatic monomers d1) and comonomers d2) and E) 0 - 40 wt. % of at least one other additive E), wherein the sum of components A) - E) amounts to 100 wt. %, in addition to methods for the production of the thermoplastic moulding compounds, the use of said thermoplastic moulding compounds in the production of moul ded bodies, films, fibers and foams, and finally said moulded bodies, films, fibres and foams which can be obtained from the thermoplastic moulding compounds.</p> |