COATED STEEL TUBE MANUFACTURING METHOD |
摘要 |
<P>PROBLEM TO BE SOLVED: To provide a coated steel tube having the excellent corrosion-resistant capacity by reducing the amount of residual air in a space formed between the outer surface of the steel tube and the inner surface of a coating material. <P>SOLUTION: When at least a part of an outer surface of a steel tube 2 is covered with a plurality of coating materials 3-7 over the entire circumference, a plurality of belts 60 are wound around outer surfaces of the wound coating materials 3-7 in a circumferential direction and bound every time one of the coating materials 3-7 is wound around the outer surface of the steel tube 2 in a circumferential direction, the wound coating materials 3-7 are fastened and fixed to the outer surface of the steel tube 2, and after the coating materials 3-7 are tightly attached to the outer surface of the steel tube 2, the primary temporary welding is performed. <P>COPYRIGHT: (C)2007,JPO&INPIT |
申请公布号 |
JP2007167933(A) |
申请公布日期 |
2007.07.05 |
申请号 |
JP20050372334 |
申请日期 |
2005.12.26 |
申请人 |
NIPPON STEEL ENGINEERING CO LTD |
发明人 |
OHIRA TAKASHI;KAWAI YASUHIRO;IWAMI HIROSHI;TACHIBANA YUICHI |
分类号 |
B21C37/15;B23K9/00;B23K11/00;B23K11/06;B23K11/11;B23K101/04;B23K101/06;E02D31/06 |
主分类号 |
B21C37/15 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|