摘要 |
<P>PROBLEM TO BE SOLVED: To provide a catalyst for oxidizing carbon monoxide, having improved long-term performance and also improved initial performance. <P>SOLUTION: The catalyst for oxidizing carbon monoxide is obtained by depositing as catalyst components, vanadium oxide, copper chloride and palladium chloride on an alumina carrier, has 60-100 m<SP>2</SP>/g specific surface area and contains chlorine of 0.5-1.4 molar ratio (Cl/(Cu+Pd)) of chlorine to copper plus palladium. <P>COPYRIGHT: (C)2007,JPO&INPIT |