摘要 |
<P>PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having extremely excellent molded material appearance, surface hardness and durability, also excellent in melt retention stability and a large-sized article-molding property, especially suitable for plumbing parts (especially, such as bath room products, wash room products, toiletry products, sink products, etc.) excellent in appearance and hardness. <P>SOLUTION: This thermoplastic resin composition is obtained by blending (C) 10-300 pts.wt. fibrous inorganic filler and/or plate-formed inorganic filler based on (X) 100 pts.wt. resin composition containing (A) 50-99 pts.wt. polytrimethylene terephthalate and (B) 50-1 pts.wt. amorphous polyester. It is preferable that the intrinsic viscosity [η] of the (A) component + (B) component is preferably 0.60-1.50 dl/g, and also (D) 0.1-20 pts.wt. styrene-based resin is contained based on 100 pts.wt. the (A) component + (B) component. <P>COPYRIGHT: (C)2007,JPO&INPIT |