摘要 To advantageously solve a problem related to thermal expansion and contraction, ferritic Cr-contained steel having a reduced thermal expansion coefficient is provided. Specifically, the ferritic Cr-contained steel contains C of 0.03% or less, Mn of 5.0% or less, Cr of 6 to 40%, N of 0.03% or less, Si of 5% or less, and W of 2.0% to 6.0% in percent by mass, and Fe and inevitable impurities as the remainder, wherein precipitated W is 0.1% or less in percent by mass, and an average thermal expansion coefficient between 20°C and 800°C is less than 12.6×10 -6 /°C.
申请公布号 EP1698711(A4) 申请公布日期 2007.06.20
申请号 EP20040808059 申请日期 2004.12.22
申请人 JFE STEEL CORPORATION 发明人 MIYAZAKI, ATSUSHI;KATO, YASUSHI;FURUKIMI, OSAMU
分类号 C22C38/00;C21D6/00;C21D8/02;C21D8/04;C21D9/46 主分类号 C22C38/00