发明名称 Method to produce an anti-swelling mica
摘要 A method to produce an anti-swelling mica having following steps: mixing powdery mica with an alkaline compound to form a mixture; heating the mixture at a temperature between 150° C.~230° C. for lasting 30 minutes to make metal ions out of the alkaline compound to diffuse into the mica homogeneously; using water to reduce temperature of the mixture so as to form an alkaline solution; separating the powdery mica from the alkaline solution to obtain a solid mica; neutralizing excessive alkaline compound adhering to the solid mica by an acid solution that is diluted by cold water and the mica anti-swells after adjusting pH of the solid mica to less than 7.0; and diluting the acid solution again by adding water and separating the solid mica from diluted acid solution to obtain a production-anti-swelling mica.
申请公布号 US7232481(B1) 申请公布日期 2007.06.19
申请号 US20060416776 申请日期 2006.05.03
申请人 CHOU MING-HUI 发明人 CHOU MING-HUI
分类号 C04B14/20;C01B33/26 主分类号 C04B14/20
代理机构 代理人
主权项
地址