摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a method for producing a laminate in which conductive thin members are laminated on both sides of a sheet-shaped substrate 60μm or below in thickness and the occurrence of wrinkles is suppressed. <P>SOLUTION: The method includes a conveyance process in which the sheet-shaped substrate 60μm or below in thickness is conveyed while tension in the conveyance direction is applied to the substrate, a first heating/pressurization process in which in order to make conductive sheet-shaped members adhere provisionally to both sides of the substrate conveyed in the conveyance process, the substrate and the conductive members are heated/pressurized simultaneously, a cutting process in which the members and the substrate laminated by the provisional adhesion in the first heating/pressurization process are cut in a prescribed length, and a second heating/pressurization process in which a plurality of the cut materials are piled and heated/pressurized simultaneously so that the members and the substrate of a cut material constituted of the members and the substrate cut in the cutting process adhere to each other. <P>COPYRIGHT: (C)2007,JPO&INPIT</p> |