POLY(ARYLENE ETHER) BLEND AND METHOD OF MAKING SAME
摘要
<p>A resin composition includes a poly(arylene ether), a poly(alkenyl aromatic) having a melt index of about 10 to about 250 grams/minute as measured by ASTM D 1238, Procedure B at 200 °C and 5 kilogram load, and a rubber-modified poly(alkenyl aromatic). The composition exhibits improved flow in extrusion and molding operations.</p>