发明名称 |
FLUORINATED ELASTOMER COMPOSITION AND METHOD FOR ITS PRODUCTION, MOLDED PRODUCT, CROSS-LINKED PRODUCT, AND COVERED ELECTRIC WIRE |
摘要 |
To provide a fluorinated elastomer composition which is excellent in flexibility, heat resistance and flame retardance, and a molded product, cross-linked product and covered electric wire, using such a fluorinated elastomer composition.;A fluorinated elastomer composition comprising a tetrafluoroethylene/propylene copolymer (a), an ethylene/tetrafluoroethylene copolymer (b), an ethylene copolymer (c) containing epoxy groups and a flame retardant (d), wherein the mass ratio [(a)/(b)] of (a) to (b) is from 70/30 to 40/60, the mass ratio [(b)/(c)] of (b) to (c) is from 100/0.1 to 100/10, and the content of (d) is from 0.1 to 30 parts by mass per 100 parts by mass of the total content of (a), (b) and (c). |
申请公布号 |
US2016196895(A1) |
申请公布日期 |
2016.07.07 |
申请号 |
US201615070459 |
申请日期 |
2016.03.15 |
申请人 |
Asahi Glass Company, Limited |
发明人 |
IRUYA Ken;YASUDA Satoko;TAGUCHI Daisuke;MATSUOKA Yasuhiko |
分类号 |
H01B3/44;C08L27/18;H01B7/295;H01B7/04;H01B7/00;B60R16/02 |
主分类号 |
H01B3/44 |
代理机构 |
|
代理人 |
|
主权项 |
1. A fluorinated elastomer composition comprising a tetrafluoroethylene/propylene copolymer (a), an ethylene/tetrafluoroethylene copolymer (b), an ethylene copolymer (c) containing epoxy groups and a flame retardant (d), wherein
the mass ratio [(a)/(b)] of the tetrafluoroethylene/propylene copolymer (a) to the ethylene/tetrafluoroethylene copolymer (b) is from 70/30 to 40/60, the mass ratio [(b)/(c)] of the ethylene/tetrafluoroethylene copolymer (b) to the ethylene copolymer (c) containing epoxy groups is from 100/0.1 to 100/10, and the content of the flame retardant (d) is from 0.1 to 30 parts by mass per 100 parts by mass of the total content of the tetrafluoroethylene/propylene copolymer (a), the ethylene/tetrafluoroethylene copolymer (b) and the ethylene copolymer (c) containing epoxy groups. |
地址 |
Chiyoda-ku JP |