摘要 |
<P>PROBLEM TO BE SOLVED: To provide a method for fabricating an optical component, in particular to provide a method for fabricating an optical compensation film used in a photoelectric flat panel display. <P>SOLUTION: A method for fabricating an optical compensation film is shown. In the process, at first, a PAR (polyarylate) is provided, the polymer is dissolved in an aprotic polar solvent to form a PAR solution, and the PAR solution is applied on a substrate, and the aprotic polar solvent contained therein is substantially removed under a predetermined temperature to form the optical compensation film having thickness of 1 to 20 μm. The optical compensation film is optically anisotropic and suitable for use in the photoelectric flat panel display. <P>COPYRIGHT: (C)2007,JPO&INPIT |