摘要 |
<P>PROBLEM TO BE SOLVED: To provide a polyarylene sulfide resin composition which forms little burr when molded, has high fluidity and excellent moldability, and has excellent mechanical strengths. <P>SOLUTION: The resin composition is prepared by compounding 100 pts.wt. polyarylene sulfide resin mixture comprising (A) 20 to 60 wt.% polyarylene sulfide resin which shows a thickening ratio of 2.0 or larger when melt-mixed with an alkoxysilane and (B) 80 to 40 wt.% polyarylene sulfide resin having a thickening ratio of 1.5 or smaller when melt-mixed with an alkoxysilane and having a number-average molecular weight of 3,000 to below 7,000 with (C) 0.1 to 3 pts.wt. an alkoxysilane compound and (D) 20 to 300 pts.wt. inorganic filler. <P>COPYRIGHT: (C)2007,JPO&INPIT |