发明名称 |
Method for work-harden of metal part by rolling, comprises pre-heating of part to strain-aging temperature |
摘要 |
<p>The metal part (2), which could be a shaft, is fixed between two revolving clamping jaws (3,4). The part (2) is heated with a suitable unit such as a heating coil (6) wound around the shaft (2). The appropriate temperature level is located within the range of strain-aging. When sufficiently heated the part (2) is rotated and a roll (8) pressed against its outer surface. The work-piece (2) can also be held stationary and the roll (8) moved around its mantle. The temperature is kept at the same level during the complete rolling process.</p> |
申请公布号 |
DE102005041250(A1) |
申请公布日期 |
2007.03.01 |
申请号 |
DE20051041250 |
申请日期 |
2005.08.29 |
申请人 |
UNIVERSITAET KASSEL |
发明人 |
ALTENBERGER, IGOR;NIKITIN, IVAN |
分类号 |
B23P9/02;B23P15/02;B24B39/02 |
主分类号 |
B23P9/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|