发明名称 Process for recovery of nickel and cobalt by heap leaching of low grade nickel or cobalt containing material
摘要 A process for the recovery of nickel and cobalt from laterite ores, the process including the steps of: a) beneficiating the ore to separate it into a beneficiated upgraded ore fraction and a coarse, siliceous low grade rejects fraction which is substantially free from fines and clay materials; b) separately processing the upgraded ore fraction for the recovery of nickel and cobalt; and c) subjecting the low grade rejects fraction to a heap leach process with an acid supplemented solution to create a heap leachate for further nickel and cobalt recovery processing.
申请公布号 US2007034056(A1) 申请公布日期 2007.02.15
申请号 US20040564358 申请日期 2004.07.13
申请人 BHP BILLITON SSM TECHNOLOGY PTY LTD 发明人 MILLER GEOFFREY W.;LIU HOUYUAN
分类号 C22B23/00;B03B5/00;B03B7/00;C22B3/04;C22B3/06;C22B3/08;C22B3/10 主分类号 C22B23/00
代理机构 代理人
主权项
地址