摘要 |
The present invention is for obtaining a silver clay that can be sintered at a low temperature, and provides a silver powder for silver clay consisting of a fine Ag powder having an average particle diameter equal to or less than 2 mu m incorporated at 15 to 50 weight %, with the remainder being an Ag powder having an average particle diameter that exceeds 2 mu m and is equal to or less than 100 mu m, and a silver clay comprising this silver powder for silver clay incorporated at 50 to 95 weight %, a binder at 0.0 to 8 weight %, an oil at 0.1 to 3 weight %, and a surface active agent at 0.03 to 3 weight %, with the remainder being water. <IMAGE> |