发明名称 |
METHOD OF PREPARING LI 1+X MN2-X O4 FOR USE AS SECONDARY BATTERY ELECTRODE |
摘要 |
A CONTINUOUS METHOD OF PREPARING A SINGLE PHASE LITHIATED MANGANESE OXIDE INTERCALATION COMPOUND OF THE FORMULA LI1+XMN2-XO4 COMPRING THE STEPS OF : MIXING INTIMATELY A LITHIUM HYDROXIDE OR A LITHIUM SALT AND A MANGANESE OXIDE OR A MANGANESE SALT; FEEDING THE INTIMATELY MIXED SALTS TO A REACTOR; CONTINUOUSLY AGITATING THE MIXED SALTS IN THE REACTOR; HEATING THE AGITATED MIXED SALTS IN THE REACTOR AT A TEMPERATURE OF FROM ABOUT 650°C TO ABOUT 800°C FOR A TIME NOT IN EXCESS FOR ABOUT 4 HOURS IN AN OXYGEN-CONTAINING ATMOSPHERE; AND COOLING THE REACTED PRODUCT TO LESS THAN ABOUT 200°C IN AN OXYGEN-CONTAINING ATMOSPHERE FOR A TIME NOT IN EXCESS OF ABOUT 2 HOURS. |
申请公布号 |
MY127833(A) |
申请公布日期 |
2006.12.29 |
申请号 |
MY1996PI04100 |
申请日期 |
1996.10.04 |
申请人 |
KERR-MCGEE CHEMICAL LLC |
发明人 |
STEPHEN W. SHEARGOLD;TERRELL N. ANDERSEN |
分类号 |
C01G45/12;C01G45/00;H01M4/131;H01M4/50;H01M4/505;H01M10/052;H01M10/36 |
主分类号 |
C01G45/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|