DEGREASING METHOD FOR ALUMINIUM HARD FOIL, ALUMINIUM HARD FOIL, ALUMINIUM HARD FOIL ELECTRODE MEMBER, AND LITHIUM ION SECONDARY BATTERY USING SAID MEMBER |
摘要 |
An aluminum hard foil is degreased without reducing the hardness to improve the coating performance of coating material. A foil-rolled aluminum foil is subjected to a low- temperature heat treatment for holding the aluminum foil at 80 to 160 0C for 1 hour or more. The low-temperature heat treatment is preferably performed by subjecting the aluminum foil to batch processing with the aluminum foil coiled. |