发明名称 SECONDARY COOLING METHOD FOR CAST SLAB IN SLAB CONTINUOUS CASTING PROCESS
摘要 PROBLEM TO BE SOLVED: To provide a secondary cooling technique capable of preventing occurrence of surface cracks and internal cracks only by improving the cooling method for cast slab without changing the component of the cast slab while keeping the productivity of a continuous caster as before. SOLUTION: The cast slab in the vertical part is cooled by an edge-off method without spraying water onto both edge parts of short sides and long sides. In this case, the edge-off amount of the long wall sides defined as [(the cast slab width)-(the spraying width)]/2 is controlled to 125 to 250 mm, and the water amount density of the cooling water sprayed to both edge parts of the long sides in the cast slab at the passing time through a bending part is controlled according to the width-cutting amount. COPYRIGHT: (C)2007,JPO&INPIT
申请公布号 JP2006315011(A) 申请公布日期 2006.11.24
申请号 JP20050136985 申请日期 2005.05.10
申请人 JFE STEEL KK 发明人 TADAMA TOMOAKI;KARIYA KAZUHIRO;KUROOKA HIROKI
分类号 B22D11/124;B22D11/22 主分类号 B22D11/124
代理机构 代理人
主权项
地址