PROBLEM TO BE SOLVED: To provide a thermoplastic resin molding which is excellent in appearance, surface hardness, scratch resistance and chemical resistance and favorably used in sanitary applications. SOLUTION: The polytrimethylene terephthalate resin molding is obtained by coating at least part of a molding with (B) a one or two pack-type curable resin composition in a film-like form and curing the resin composition (B). The molding is composed of a resin composition which is obtained by blending 0-150 pts.wt. of (A4) an inorganic filler with 100 pts.wt. of the aggregate of 99-50 pts.wt. of (A1) a polytrimethylene terephthalate resin, 0-50 pts.wt. of (A2) a thermoplastic resin and 0-20 pts.wt. of (A3) an epoxy resin. COPYRIGHT: (C)2007,JPO&INPIT
|