摘要 |
PROBLEM TO BE SOLVED: To provide a transparent conductive film laminate and its manufacturing method wherein curling and deformation prevention of a base material, and peeling-off prevention and attainment of low resistance of the transparent conductive film are enabled. SOLUTION: The transparent conductive film is formed on at least one face of the base material, the transparent conductive film has a laminated constitution of at least one layer or more, the transparent conductive film is applied of an annealing treatment by ultraviolet irradiation to every layer, and the transparent conductive film is made to be the transparent conductive film laminate in which X-ray diffraction peaks caused by a crystal in which amorphous state is not mixedly existing are observed at all parts of the inside of the film. COPYRIGHT: (C)2007,JPO&INPIT
|