发明名称 Process for casting a Titanium-alloy
摘要 <p>To cast a beta -titanium alloy, containing 7.5-20.0% molybdenum, the alloy is melted at a temperature of >=1770[deg]C to be poured with fine casting into a mold with hot isostatic pressure. The molding is annealed and finally quenched.</p>
申请公布号 EP1696043(A1) 申请公布日期 2006.08.30
申请号 EP20050004173 申请日期 2005.02.25
申请人 WALDEMAR LINK GMBH & CO. KG 发明人 BALIKTAY, SEVKI
分类号 C22C14/00;C22F1/18 主分类号 C22C14/00