A method for obtaining of a coating includes application on the metallic surface of the composition, which contains 34- 40% solution in organic solvent of polymethylphenylsiloxane resin and filler, which contains the mixture of soot, lignin modifier of the rust MRL-91, aluminum powder, taken in the mass ratio of (43-55):(37-50):(5-10) respectively, and drying of obtained coating. After drying of the obtained coating 34-40% solution in organic solvent of polymethylphenylsiloxane resin is applied. The drying of coating is carried our at 100-140 DEGREE C for 0.5 hours, and after drying 34-40% solution in organic solvent of polymethylphenylsiloxane resin is applied, the drying is carried out at a temperature of 410-450 DEGREE C for 3.5-4 hours.
|