摘要 |
Method for producing silicon carbide fibers by mixing discontinuous isotropic carbon fibers with a silica source and exposing the mixture to a temperature of from about 1450° C. to about 1800° C. The silicon carbide fibers are essentially devoid of whiskers have excellent resistance to oxidation and excellent response to microwave energy, and can readily be formed into a ceramic medium employing conventional ceramic technology. The fibers also may be used for plastic and metal reinforcement.
|