摘要 |
FIELD: medicine. ^ SUBSTANCE: the present innovation is directed to obtain a covering that provides high ability for developing bony tissue. This result should be fulfilled due to applying suspension upon titanium and its alloys with direct or impulse current under conditions of spark discharge, drying at about 80-120° C and roasting at about 600-800° C for 0.5-1 h, where as suspension one should apply synthetic and biological hydroxyapatite powder at the following quantitative ratio of components, weight%: synthetic hydroxyapatite powder 10-90, biological hydroxyapatite powder 10-90. ^ EFFECT: higher efficiency. ^ 2 dwg, 3 ex, 1 tbl |